Thornel® Graphite Cloth

 

Subcategory: Carbon Fiber; Graphite; Carbon

Close Analogs: Thornel® products were sold by Amoco and are now owned by Cytec.

Key Words: Carbon Fiber; Carbon Fibre; BP Amoco Performance Products, Inc.

Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc.

Carbon and graphite cloths, consisting entirely of flexible filaments, are produced by pyrolysis of rayon cloth at high temperatures to yield products with a high degree of purity. The cloth flexibility results from the very small filament diameter. These are fair conductors of electricity. At room temperature the volume resistivity of graphite cloth is about 40 times that of "Nichrome" wire. Graphite cloth resistance decreases with temperature, reaching half of the room temperature value at 1315°C.

99.9% carbon assay, 8.9 µm filament diameter

Available Properties
  • Density
  • Specific Surface Area
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Electrical Resistivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Inert
  • Emissivity (0-1)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。