Toho Besfight® G50-300 12K HMA-7C EP01 Continuous Filament Carbon Fiber
Subcategory: Carbon Fiber; Carbon
Material Notes: High Modulus; Collimated; Polyacrlonitrile (PAN) based fiber Typical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.
| Available Properties |
- Density
- Fiber Count
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Electrical Resistivity
- Filament Diameter
- Size Level
|
|
|
|