Tenax Pyromex® Tow CPX 2d 312K Non-crimped Carbon Fiber
Subcategory: Carbon Fiber; Carbon
Material Notes: Pyromex® is an oxidized organic polyacrlonitrile (PAN) fiber with excellent heat and flame resistance. It also features excellent resistance to chemicals and good electrical insulation properties. In addition, unlike inorganic fibers, this yarn is highly processible for yarn spinning and weaving. Pyromex® is widely used in anti-spattering sheets for welding, fleeces or needle felts for heat protection in the auto or aerospace industries, heat protective clothing, protective covering for furnaces, heat insulators, brake or clutch discs, and high temperature carbon/carbon composite (C/C) parts. It is available as tow or staple fiber. Information provided by Toho Carbon Fibers, a wholly owned subsidiary of Toho Tenax Co., Ltd.
| Available Properties |
- Density
- Water Absorption at Saturation
- Fiber Count
- Tenacity
- Elongation at Break
- Finish
- Number of Filaments
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|