Ultracor® UCF-355-3/8-3.5 Honeycomb Core Material

 

Key Words: Carbon Fiber Composite Core Material; Carbon T300

Material Notes:
Construction: ±45° T300. Fiber: Carbon T300. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be used in spacecraft Antenna Reflectors, Optical Benches, Solar Arrays, and other lightly loaded structures which must be positioned with accuracy and stability in order to properly perform their intended purpose. It was developed using a space qualified, toughened, polycyanate matrix resin. General Ultracor® features include low density, design flexibility, low CTE, low CME, and high thermal conductivity.

Data provided by Ultracor Inc., formerly YLA Cellular Products Company.

Available Properties
  • Density
  • Compressive Yield Strength
  • Compressive Modulus
  • Shear Modulus
  • Shear Strength
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。