AISI 1006 Steel, cold drawn bar, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G10060, ASME 5041, ASTM A29, ASTM A510, ASTM A545, FED QQ-W-462, MIL SPEC MIL-S-11310 (CS1006), SAE J403, SAE J412, SAE J415
Material Notes: The composition shown above is for structural shapes, plates, strip, sheets, and welded tubing only. Semifinished products for forging, hot-rolled and cold finished bars, wire rods, and seamless tubing have a magnesium range of 0.25 - 0.40%. Applications: Soft, very ductile, used in applications which require severe bending and welding such as panels for automobiles or appliances. Also used in magnet core applications.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|