AISI 1008 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G10080, JIS G3141(96) SPCC, ASTM A29, ASTM A108, ASTM A510, ASTM A512, ASTM A513, ASTM A519, ASTM A545, ASTM A575, ASTM A576, ASTM A619, ASTM A620, ASTM A621, ASTM A622, ASTM A635, FED QQ-S-637 (C1008), FED QQ-S-698 (C1008), FED QQ-W-461, MIL SPEC MIL R-8814, MIL SPEC MIL S-11310 (CS1008,1008), SAE J1397, SAE J403, SAE J412, SAE J414, DIN 1.0204, UNI CB10 FU
Material Notes: Usually produced as rimmed, capped, semikilled, and fully killed, Rimmed have exceptional cold fomability. Weldability (spot, projection, butt, and fusion) and brazeability are excellent. Applications include extruded, cold headed, cold upset, and cold pressed parts and forms.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|