AISI 1010 Steel, hot rolled bar, 19-32 mm (0.75-1.25 in) round or thickness
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G10100, AMS 5040, AMS 5042, AMS 5044, AMS 5047, AMS 5053, ASTM A29, ASTM A108, ASTM A510, ASTM A519, ASTM A545, ASTM A549, ASTM A575, ASTM A576, MIL SPEC MIL-S-11310 (CS1010), JIS S 9 CK, SAE J403, SAE J412, SAE J414, DIN 1.1121, AFNOR XC 10 (Fr), JIS S10 C, JIS S 12 C
Material Notes: Easily cold formed by heading, extruding, upsetting, bending, and other deforming processes. Uses for wires include electroplated products, such as racks, storage bins, shopping carts, fan guards, and jewelry, and unplated such as wires, staples, hardware, and barbed wire.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|