AISI 1012 Steel, CQ sheet,1.6-5.8 mm round or thickness
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G10120, ASTM A29, ASTM A510, ASTM A519, ASTM A545, ASTM A549, ASTM A575, ASTM A576, MIL SPEC MIL-S-11310 (CS1012), SAE J403, SAE J412, SAE J414
Material Notes: Easily cold formed by heading, extruding, upsetting, bending, and other deforming processes. Uses for wires include electroplated products, such as racks, storage bins, shopping carts, fan guards, and jewelry, and unplated such as wires, staples, hardware, and barbed wire.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|