AISI 1015 Steel, mock carburized at 915°C (1680°F) for 8 hours, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper, 25 mm (1 in.) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G10150, AMS 5060, ASTM A29, ASTM A108, ASTM A510, ASTM A545, ASTM A549, ASTM A575, ASTM A576, ASTM A659, FED QQ-S-698 (C1015), MIL SPEC MIL-S-16974, SAE J403, JIS S 17 C, JIS S 15 CK, SS14 1370 (Sweden), SAE J412, SAE J414, DIN 1.1141, AFNOR XC 15 (Fr), AFNOR XC 18 (Fr), JIS S 15 C
Material Notes: Better machinability and carburizing. Can be strengthened by cold working or surface hardened by carburizing or cyaniding. Hot rolled sheet has excellent weldability. Post water quenched hardness: 99 HRB surface, 91 HRB half-radius, 90 HRB Center.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|