AISI 1016 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round

 

Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal

Close Analogs: AISI 1017, AISI 1018, AISI 1019

Key Words: UNS G10160, ASTM A29, ASTM A108, ASTM A510, ASTM A513, ASTM A545, carbon steels, ASTM A548, ASTM A549, ASTM A576, ASTM A659, MIL SPEC MIL-S-866, SAE J403, SAE J412, SAE J414, DIN 1.0419, DIN 1.1142, DIN GS-Ck16, DIN RSt44.2, DIN 17115 1.0467, DIN 17115 1.0468, DIN 17115 15Mn3, DIN 17115 15Mn3Al, BS 3059 440, BS 3606 440, BS 970 080A15, BS 970 080M15, BS 970 170H15, BS 970 173H16, EN32

Material Notes:
Supplied as killed, semikilled, rimmed, and capped steel. Good weldability, relatively soft and strengthen with cold work during forming or drawing. Widely used in cold forming operations such as heading, upsetting, and extrusion. Used in the as-rolled condition as bar, shapes, sheet, and strip.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell B
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Bulk Modulus
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • Electrical Resistivity at Elevated Temperature
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Specific Heat Capacity at Elevated Temperature
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。