AISI 1017 Steel, cold drawn
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 1016, AISI 1018, AISI 1019
Key Words: AFNOR NF A35-556 XC18, AIR 9160-C21 9160C011, DIN 17210 1.1141, DIN 17210 Ck15, MSZ 500 B38 X (Hungary), AFNOR XC15, AFNOR NF A35-551 XC18, AFNOR NF A35-552 XC18, AFNOR NF A35-553 XC18S, AFNOR NF A35-554 XC18S, carbon steels, UNS G10170, ASTM A29 1017, ASTM A29 M1017, ASTM A510 1017, ASTM A513 1017, ASTM A519 1017, ASTM A575 M1017, ASTM A635 1017, ASTM A659 1017, ASTM A830 1017, MIL-S-11410 1017, MIL S-11410 CS1017, BDS 2592 BSt3kp (Bulgaria), BDS 2592 BSt3ps, BDS 2592 BSt3sp, BDS 9801 VSt3kp, BDS 9801 VSt3ps, BDS 9801 VSt3sp, BDS 9801 WSt3kp, BDS 9801 WSt3ps, BDS 9801 WSt3sp, GB 714 A3q (China), GB 900 B3, GB 900 B3F, GB 900 C3, GB 300 C3F, JIS S15C, JIS S15CK, JIS G4051 S17C, DGN B-301 1017 (Mexico), COPANT 333 1017, STAS 10607 16 (Romania), PN 84023 18A (Poland), PN 84023 St3NO, PN 84024 R45, PN 84024 R45A, PN 84024 St44K, SAE J1397 1017, SAE J403 1017, SAE J412 1017, ONORM M3110 RC15 (Australia), NBN 253-03 C16-2 (Belgium)
Material Notes: Medium-low carbon steels have good weldability and slightly better machinability than the lower carbon steels. Relatively soft and strengthen with cold work during forming or drawing
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|