AISI 1018 Steel, carburized at 925°C (1700°F), box cooled, 775°C (1430°F) reheat, water quenched, 175°C (350°F) temper. 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 1016, AISI 1017, AISI 1019
Key Words: UNS G10180, AMS 5069, ASTM A29, ASTM A108, ASTM A510, ASTM A513, ASTM A519, ASTM A544, ASTM A545, ASTM A548, ASTM A549, ASTM A576, ASTM A659, AS 1442 K1018 (Australia), AS 1443 K1018, CSN 12020 (Czech), CSN 12022, AFNOR NF A33-101 AF42C20, DIN 1.0453, DIN C16.8, DGN B-301 1018 (Mexico), COPANT 331 1018 (Pan America), COPANT 333 1018, MIL SPEC MIL-S-11310 (CS1018), SAE J403, SAE J412, SAE J414, MST.T (Russia), ST.20A, ST.3, ST.3T, GOST M18S, GOST 23570 18ps, GOST 23570 18sp, GOST 5520 18K, GOST 5521 S, NBN 629 D37-2 (Belgium), NBN 630 E37-1, NBN 630 E37-2, NBN A21-221 C17KD, BDS 9801 S (Bulgaria), GB 715 ML3 (China), TS 302 Fe35.2 (Turkey), TS 346 Fe35, BS 970 080A17, DEF STAN95-1-1 C1018
Material Notes: Supplied as killed, semikilled, rimmed, and capped steel. Good weldability, relatively soft and strengthen with cold work during forming or drawing. Widely used in cold forming operations such as heading, upsetting, and extrusion. Used in the as-rolled condition as bar, shapes, sheet, and strip.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|