AISI 1019 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 1016, AISI 1017, AISI 1018
Key Words: SAE J403, SAE J412, SAE J414, SAE J1397, FED QQ-S-633, MIL R-6532, MIL R-908, MIL-S-12505, MIL-S- 16113, MIL-S-20166, UNS G10190, ASTM A29, ASTM A510, ASTM A513, ASTM A519, ASTM A545, ASTM A548, ASTM A576, ASTM A635, ASTM A830
Material Notes: Supplied as killed, semikilled, rimmed, and capped steel. Good weldability, relatively soft and strengthen with cold work during forming or drawing. Widely used in cold forming operations such as heading, upsetting, and extrusion. Used in the as-rolled condition as bar, shapes, sheet, and strip.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|