AISI 1020 Steel, normalized at 870°C (1600°F)
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G10200, AMS 5032, AMS 5045, ASTM A29, ASTM A108, ASTM A510, ASTM A519, ASTM A29, A108, A510, A512, A513, A519, A544, A575 M10120, A576, A635, A659, A827, A830, BS 970 040A20, 050A20 (En2C), 050A20 (En2D), 060A20, BS 970 Part 1 070M20, DEF STAN95-1-1 C1020, SAE J412, SAE J414, DIN 1.0402, AFNOR CC 20, UNI C 20, SS14 1450 (Sweden), SAE J403
Material Notes: Applications include parts in the case hardened condition where core strength is not critical, and for shafts of larger cross section that are not highly stressed. Other uses include lightly stressed gears with hard wearing surfaces and case hardened pins and chains.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Charpy Impact
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|