AISI 1026 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 1023, AISI 1025
Key Words: UNS G10260, ASTM A29, ASTM A273, ASTM A510, ASTM A519, ASTM A545, ASTM A576, carbon steels
Material Notes: Similar to 1020 steel, responds well to heat treating and cold work. Fair machinability and weldability. Excellent cold formability.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|