AISI 1030 Steel, as rolled
Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 1034, AISI 1035
Key Words: SAE J414, ASTM A108; ASTM A29;ASTM A510; ASTM A512; ASTM A519; ASTM A544; ASTM A545; ASTM A546; ASTM A576; ASTM A682, DIN 1.1172; FED QQ-S-635 (C1030); FED QQ-S-700 (C1030); MIL SPEC MIL-S-11310 (CS1030); SAE J403; SAE J412
Material Notes: The Iron content above is a typical value and in actuality should be calculated as a remainder. Moderate strength and hardness in the as-rolled condition. Fair machinability and weldability. Precautions must be taken when welding to avoid cracking during cooling.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|