AISI 1030 Steel, normalized 925°C (1700°F)
Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 1034, AISI 1035
Key Words: UNS G10300, ASTM A29, ASTM A108, ASTM A510, ASTM A512, ASTM A519, ASTM A544, carbon steels
Material Notes: The Iron content above is a typical value and in actuality should be calculated as a remainder. Moderate strength and hardness in the as-rolled condition, can be strengthened and hardened by cold work. Fair machinability and weldability.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|