AISI 1030 Steel, annealed at 845°C (1550°F), furnace cooled 11°C (20°F) per hour to 650°C (1200°F), air cooled, 25 mm (1 in.) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 1034, AISI 1035
Key Words: UNS G10300, ASTM A29, ASTM A108, ASTM A510, ASTM A512, ASTM A519, ASTM A544, carbon steels, ASTM A545, ASTM A546, ASTM A576, ASTM A682, FED QQ-S-635 (C1030), FED QQ-S-700 (C1030), MIL SPEC MIL-S-11310 (CS1030), SAE J403, SAE J412, SAE J414, DIN 1.1172, UNI CB 35
Material Notes: The Iron content above is a typical value and in actuality should be calculated as a remainder. Applications include levers, bolts, studs, nuts, and similar parts which are headed, upset, or extruded. Wires uses include nails requiring high shank rigidity or strength and quench-hardened nails. Post water quenched hardness: 46 HRC surface, 23 HRC half-radius, 21 HRC surface
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|