AISI 1034 Steel
Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 1030, AISI 1035
Key Words: AFNOR XC 38, JIS S 38 C, carbon steels, UNS G10340, ASTM A29, ASTM A181, SAE J118, SAE J412, DIN 1.1181, AFNOR XC 32, AFNOR XC 35
Material Notes: This AISI/SAE steel was discontinued as a standard in 1968. Water-hardening steels suitable for small parts of moderate strength. Used in levers, bolts, nuts, studs and similar parts which are headed, upset, or extruded. This steel deleted as a SAE-AISI standard in 1968.
| Available Properties |
- Density
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|