AISI 1039 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal
Key Words: UNS G10390, ASTM A29, ASTM A510, ASTM A546, ASTM A576, SAE J403, SAE J412, B.S. CDS105/106 (U.K), SAE J414, DIN 1.1157, AFNOR 35 M 5, B.S. 120 M 36, B.S. 150 M 36
Material Notes: Typical uses include machine, plow, and carriage bolts, tie wire, cylinder head studs, and machined parts, U-bolts, concrete reinforcing rods, forgings, and non-critical springs.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|