AISI 1044 Steel, merchant quality, hot rolled, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal
Key Words: UNS G10440, ASTM A29, ASTM A510, ASTM A575, ASTM A576, SAE J403, SAE J412, SAE J414
Material Notes: Respond to heat treatment, and flame and induction hardening, but not recommended for carburizing or cyaniding. Die forging and hot upsetting are good to excellent. Typical uses include gears, shafts, axles, bolts, studs, and machine parts.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|