AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

 

Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal

Close Analogs: AISI 1045H

Key Words: AFNOR NF A35-553 XC45, AFNOR NF A35-554 XC48, DIN 1654 1.1192, DIN 1654 Cq45, DIN 17200 1.0503, AFNOR XC42, AFNOR XC42TS, AFNOR XC48TS, AFNOR NF A33-101 AF65C45, AFNOR NF A35-552 XC48H1, UNS G10450, ASTM A29, ASTM A108, ASTM A266 Class 3, ASTM A304, ASTM A311, ASTM A510, ASTM A519, AS 1442 K1045 (Australia), AS 1442 S1045, AS 1443 K1045, AS 1443 S1045, AS 1446 K1045, AS 1446 S1045, ASTM A568, ASTM A576, ASTM A682, ASTM A827, ASTM A830, FED QQ-S-635, FED QQ-S-700, FED QQ-W-461, MIL S-24093, MIL S-3039, BDS 6354 45G2A, BDS 6354 45G2K2, BDS 6354 45G2K3, GB 3078 45 (China), GB 3088 45, GB 699 45, YB 6 45B, DIN 17200 1.1191, DIN 17200 1.1201, DIN 17200 C45, DIN 17200 CK45, DIN 17200 Cm45, DIN 17200 GS-CK45, DIN 17212 1.1193, MIL S-46070, SAE J1397, SAE J403, SAE J412, BS 970 Part 1 O60A47 (U.K), BS 970 Part 1 080A47, BS 970 Part 1 080M46, NBN 253-02 C45-3, NBN 253-06 C46, BDS 3492 45LI (Bulgaria), BDS 3492 45LII, BDS 3492 45LIII, BDS 5785 45, BDS 6354 45G2, ONORM M3108 C45SW (Austria), ONORM M3110 RC45, ONORM M3161 C45, NBN 253-02 C45-1 (Belgium), NBN 253-02 C45-2

Material Notes:
Medium-carbon steel, can be hammer forged. Can be heat treated, flame or induction hardened, but not recommended for carburizing or cyaniding. AISI cross reference for JIS S45C and KS SM45C.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell B
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Bulk Modulus
  • Poissons Ratio
  • Machinability
  • Shear Modulus
  • Electrical Resistivity
  • Electrical Resistivity at Elevated Temperature
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Specific Heat Capacity at Elevated Temperature
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。