AISI 1055 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; High Carbon Steel; Metal
Key Words: UNS G10550, ASTM A29, ASTM A510, ASTM A576, ASTM A682, FED QQ-S-700 (C1055), EN43C, SAE J403, SAE J412, SAE J414, DIN 1.1209
Material Notes: Applications include battering tools, hot upset forging dies, ring-rolling tools, wear-resistant parts, hand tools, and parts for agricultural implements which require high strength at low cost. When heat treated, this steel yields a high surface hardness, combined with good toughness. Good forging characteristics.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|