AISI 1050 Steel, annealed at 790°C (1450°F), furnace cooled 10°C (18°F) per hour to 650°C (1200°F), air cooled, 25 mm (1 in.) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal
Key Words: UNS G10500, AMS 5085, ASTM A29, ASTM A510, ASTM A519, ASTM A576, ASTM A682, DIN 1.1210, JIS S 53 C, JIS S 55 C, FED QQ-S-635 (C1050), FED QQ-S-700 (C1050), MIL SPEC MIL-S-16974, SAE J403, SAE J412, SAE J414
Material Notes: The composition listed above applies only to structural shapes, plates, strip, and welded tubing. Semifinished products for forging, hot-rolled and cold-finished bars, wire rods, and seamless tubing have carbon ranges of 0.48 - 0.55%.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|