AISI 1064 Steel, cold drawn, spheroidized, annealed, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; High Carbon Steel; Metal
Key Words: UNS G10640
Material Notes: High-carbon steel, good for wire which exhibits a high tensile strength and is heat treatable. Spring wire that is untempered spheroidized annealed in process, or spheroidized annealed at finished size, requires careful control of the composition to ensure a uniform response to the heat treatment.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|