AISI 1064 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; High Carbon Steel; Metal
Key Words: UNS G10640, ASTM A26, ASTM A29, ASTM A57, ASTM A230, ASTM A682, SAE J403, SAE J412, SAE J414, DIN 1.221, AFNOR XC 60 (Fr), AFNOR XC 65 (Fr), SS14 1665 (Sweden), SS14 1678 (Sweden)
Material Notes: Applications include springs for upholstered furniture and automotive seats and backs.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|