AISI 1070 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; High Carbon Steel; Metal
Key Words: UNS G10700, AMS 5115, ASTM A29, ASTM A510, ASTM A576, ASTM A682, MIL SPEC MIL-S-11713 (2), SAE J403, SAE J412, SAE J414, DIN 1.1231, AFNOR XC 68 (Fr), SS14 1770 (Sweden), SS14 1778 (Sweden)
Material Notes: Applications include springs for upholstered furniture and automotive seats and backs.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|