AISI 1074 Steel, hot rolled
Subcategory: Carbon Steel; AISI 1000 Series Steel; High Carbon Steel; Metal
Key Words: UNS G10740, AMS 5120 D, ASTM A29, ASTM A682, FED QQ-S-700 (C1074), MIL SPEC MIL-S-46049, SAE J403, SAE J412, SAE J414
Material Notes: Good for high strength, heat treatable wire. Applications: springs for upholstered furniture and automotive seats and backs. This steel was deleted as a SAE-AISI standard in 1993.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|