AISI 1080 Steel, annealed at 790°C (1450°F), furnace cooled 11°C (20°F) per hour to 650°C (1200°F), air cooled, 25 mm (1 in.) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; High Carbon Steel; Metal
Key Words: UNS G10800, AMS 5110, ASTM A29, ASTM A510, ASTM A576, ASTM A682, FED QQ-S-700 (C1080), MIL SPEC MIL-S-16974, SAE J403, SAE J412, SAE J414
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|