AISI 1095 Steel, oil quenched 800°C (1470°F), 480°C (900°F) temper, 100 mm (4 in.) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; High Carbon Steel; Metal
Key Words: UNS G10950, AMS 5121, AMS 5122, AMS 5132, AMS 7304, ASTM A29, ASTM A510, ASTM A576, ASTM A682, FED QQ-S-700 (C1095), MIL SPEC MIL-S-16788 (C10), SAE J403, SAE J412, SAE J414, DIN 1.1274, JIS SUP 4, SS14 1870 (Sweden), B.S. 060 A 96, B.S. EN 44 B
Material Notes: Applications include edge tools, wear-resistant parts, high-stress flat springs, hot coiled springs, plow beams, plow shares, scraper blades, discs, mower knives, and harrow teeth. Post oil quenched hardness: 40 HRC surface, 37 HRC half-radius, 30 HRC center
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|