AISI 11L17 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Material Notes: Iron content calculated as remainder. Lead addition inproves the machinability of 11L17 versus 1117. Manganese content leads to increased hardenability. Used where case hadenability and good machinability are needed, such as in medium duty shafts, studs, pins, and universal joints.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|