AISI 1137 Steel, oil quenched from 855°C (1570°F), 595°C (1100°F) temper, 13 mm (0.5 in.) round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel; Metal
Key Words: UNS G11370, AMS 5024 C, ASTM A29, ASTM A108, ASTM A311, FED QQ-S-637 (C1137), SAE J403, SAE J412, SAE J414
Material Notes: Medium strength and good machinability. Applications include spline shafts, and studs, bolts, and nuts with machined threads. Post oil quenched hardness: 48 HRC surface, 43 HRC half-radius, 42 HRC center.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Izod Impact
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|