AISI 1212 Steel, cold drawn, 19-38 mm round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 1211, AISI 1213, AISI 1215
Key Words: UNS G12120, AMS 5010 D, ASTM A29, ASTM A108, FED QQ-S-637 (C1212), SAE J404, DIN 1.0711, UNI 10 S 20, JIS SUM 21, ISO 683, ISO 683/IX
Material Notes: Typical applications are frequently rolled into rods, then drawn into wire. This wire is straightened, cut to length, and used in screw machine operations. This steel series are both rephosphorized and resulfurized.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|