AISI 1215 Steel, drawn, ground, and polished, 19-38 mm round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 1211, AISI 1212, AISI 1213
Key Words: UNS G12150, ASTM A29, ASTM A108, FED QQ-S-637, SAE J412, ISO 683, ISO 683/IX
Material Notes: Typical applications are frequently rolled into rods, then drawn into wire. This wire is straightened, cut to length, and used in screw machine operations. This steel series are both rephosphorized and resulfurized.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|