AISI 12L13 Steel, cold drawn, 19-38 mm round
Subcategory: Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G12134, ASTM A29, FED QQ-S-633(C12l13), MIL SPEC MIL-S-18411, SAE J403, JIS SUM 24 L, SS14 1914 (Sweden), SAE J412, DIN 1.0718, UNI 9SMnPb23, JIS SUM 22 L, JIS SUM 23 L
Material Notes: Applications include high-speed screw machine products where superior machining characteristics of this steel can be fully utilized.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|