AISI 1330 Steel
Subcategory: Low Alloy Steel; AISI 1000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 1330H
Key Words: UNS G13300, ASTM A322, ASTM A331, ASTM A519, MIL SPEC MIL-S-16974, SAE J404, SAE J440, SAE J770, DIN 1.1165, JIS SMn 1 H, JIS SCMn 2
Material Notes: Applications for hot rolled bar include construction and machining into components; cold finished bar is suitable for heat treatment, machining into components, or constructional applications.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|