AISI Grade 18Ni (200) Maraging Steel, solution annealed at 815°C (1500°F) for 1 hour, air cooled, aged at 480°C (900°F) for 3 hours, tested at 315°C (600°F)
Subcategory: Low Alloy Steel; Maraging Steel; Low Carbon Steel; Metal
Key Words: maraging steels, UNS K92810, ASTM A538 (A), ASTM A579 grade 71
Material Notes: Applications: Bearings, Belleville springs, bolts, cannon recoil springs, rocket motor and missiles cases, couplings, load cells, flexures for guidance mechanisms of missiles, helicopter drive shafts, transmission shafts, fan shafts in commercial jet engines, aircraft wing components and forgings, aluminum die casting dies, cold forming dies, plastic molding dies, cores, pins, punches, and trim knees.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 500°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|