AISI 4024 Steel
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G40240, ASTM A29, ASTM A29M, ASTM A322, ASTM A331, ASTM A519, ASTM A752, SAE 770, SAE J404, SAE J412, SAE J770
Material Notes: Sulfur content for SAE 770 is 0.04-0.05 - SAE 770(84) 4024 is an obsolete specification; refer to J1397(92) 4024. Carburizing temperature: 900-925°C (1650-1700°F) Normalizing temperature: >= Carbarizing temperature and air cooled. Quenched in oil.
Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|