AISI 4027 Steel, water quenched 865°C (1590°F), 595°C (1100°F) temper, 14 mm (0.55 in.) round
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G40270, ASTM A322, ASTM A331, ASTM A519, SAE J404, SAE J412, SAE J770, alloy steels
Material Notes: As quenched hardness: 50 HRC surface, 50 HRC 1/2 radius, 50 HRC center.
Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
|