AISI 4037 Steel
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal
Key Words: alloy steels, UNS G40370, ASTM A322, ASTM A331, ASTM A519, ASTM A547, SAE J404, SAE J412, SAE J770
Material Notes: Oil quenched. Forging temp.: 1230 °C (2250°F) max. Annealing temp.: 830°C - 925°C (max. hardness 183 HB). Normalizing temp.: 855 - 955°C (approx. hardness 235 HB). Hardening temp.: 830 - 855°C
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|