AISI 4118 Steel, normalized at 910°C (1670°F), air cooled, 14 mm (0.55 in.) round
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Close Analogs: AISI 4148H
Key Words: alloy steels, UNS G41180, ASTM A322, ASTM A331, ASTM A505, ASTM A519
Material Notes: Normalized: heated to 910°C (1670°F), air cooled. Oil quenched. Forging temp.: 1230°C (2250°F) max. Carburizing temp.: 885 - 925°C. Hardening temp.: 830°C. Tempering temp.: 120 - 185°C.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|