AISI 4118 Steel, direct quenched from pot, carburized, 230°C (450°F) temper
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Key Words: alloy steels, UNS G41180, ASTM A322, ASTM A331, ASTM A505, ASTM A519
Material Notes: Heat treatment: Direct quench from pot, carburized at 925°C for 8 hrs., quenched in agitated oil, 230°C (450°F) temper, 1.6 mm case depth.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Fatigue Strength
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|