AISI 4135 Steel
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 4135H
Key Words: alloy steels, UNS G41350, AMS 6365C, AMS 6372C, ASTM A711, ASTM A355, ASTM A519
Material Notes: Oil quenched. Forging temp.: 1205°C (2200°F) max. Annealing temp.: 790 - 845°C. Hardening temp.: 845 - 870°C. Tempered to desired hardness.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |