AISI 4130H Steel, water quenched 855°C (1570°F), 595°C (1100°F) temper, 100 mm (4 in.) round
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 4130
Key Words: AFNOR 25 CD 4, JIS SCM2, JIS SCCrM 1, SS14 2225 (Sweden), alloy steels, UNS H41300, ASTM A304, SAE J1268, DIN 1.7218
Material Notes: Post water quenched hardness: 45.5 HRC surface, 25 HRC 1/2 radius, 24.5 center.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- Specific Heat Capacity
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|