AISI 4140 Steel, oil quenched, 13 mm (0.5 in.) round [845°C (1550°F) quench, 540°C (1000°F) temper]

 

Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal

Close Analogs: AISI 4140H

Key Words: AFNOR 40 CD 4, AFNOR 42 CD 4 (France), ASTM A322, ASTM A331, ASTM A505, ASTM A519, ASTM A646, B.S. 708 A 42 (UK), B.S. 708 M 40 (UK), B.S. 709 M 40 (UK), JIS SCM 4 H, JIS SCM 4, SS14 2244 (Sweden), MIL SPEC MIL-S-16974, SAE J404, SAE J412, SAE J770, DIN 1.7225, UNS G41400, AMS 6381, AMS 6382, AMS 6390, AMS 6395, IS 1570 40Cr1Mo28, IS 4367 40Cr1Mo28, IS 5517 40Cr1Mo28

Material Notes:
As quenched hardness after oil quenching: Surface - 57 HRC, 1/2 radius - 56 HRC; Center - 55 HRC

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell B
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Bulk Modulus
  • Poissons Ratio
  • Machinability
  • Shear Modulus
  • Electrical Resistivity
  • Electrical Resistivity at Elevated Temperature
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity at Elevated Temperature
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。