AISI 4140 Steel, oil quenched, 25 mm (1 in.) round (845°C (1550°F) quench, 595°C (1000°F) temper)
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 4140H
Key Words: ASTM A322, ASTM A331, ASTM A505, ASTM A519, ASTM A646, B.S. 708 A 42 (UK), B.S. 708 M 40 (UK), B.S. 709 M 40 (UK), JIS SCM 4 H, JIS SCM 4, SS14 2244 (Sweden), MIL SPEC MIL-S-16974, SAE J404, SAE J412, SAE J770, DIN 1.7225, UNS G41400, AMS 6381, AMS 6382, AMS 6390, AMS 6395, UNS H41500, ASTM A304, SAE J1268, DIN 1.7228, JIS SCM 5, JIS SCM 5 H, IS 1570 40Cr1Mo28, IS 4367 40Cr1Mo28, IS 5517 40Cr1Mo28
Material Notes: As quenched hardness after oil quenching: Surface - 55 HRC, 1/2 radius - 55 HRC; Center - 50 HRC
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity at Elevated Temperature
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|