AISI 4150H Steel, oil quenched 830°C (1525°F), 540°C (1000°F) temper, 25 mm (1 in.) round
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal
Close Analogs: AISI 4150
Key Words: Chromium-molybdenum steels, UNS H41500, ASTM A304, SAE J1268, DIN 1.7228, JIS SCM 5, JIS SCM 5 H
Material Notes: Post oil quenched hardness: 62 HRC surface, 62 HRC 1/2 radius, 62 HRC center
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|