AISI 4419 Steel, mock carburized, 230°C (450°F) temper, 14 mm (0.55 in.) round
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G44190, ASTM A322, ASTM A331, SAE J404, SAE J412, SAE J770
Material Notes: Mock carburized 925°C (1700°F) for 8 hrs., reheated to 845°C (1550°F), oil quenched, 230°C (450°F) temper, 14 mm round
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|