AISI 4320 Steel, double quenched and tempered (carburized 925°C (1700°F) for 8hrs, pot cooled, reheated to 815°C (1500°F), quenched in agitated oil, reheated to 775°C, quenched in agitated oil, 230°C (450°F) temper), 230°C (450°F) temper
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Low Carbon Steel; Metal
Key Words: UNS G43200, ASTM A322, ASTM A331, ASTM A505, ASTM A519, ASTM A535
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell B
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|