AISI 4340 Steel, oil quenched 855°C (1570°F), 230°C (450°F) temper for 4 hrs., tested at -255°C (-430°F)
Subcategory: Low Alloy Steel; AISI 4000 Series Steel; Medium Carbon Steel; Metal
Key Words: alloy steels, UNS G43400, AMS 5331, AMS 6359, AMS 6414, AMS 6415, ASTM A322, ASTM A331, ASTM A505, ASTM A519, ASTM A547, ASTM A646, MIL SPEC MIL-S-16974, B.S. 817 M 40 (UK), SAE J404, SAE J412, SAE J770, DIN 1.6565, JIS SNCM 8, IS 1570 40Ni2Cr1Mo28, IS 1570 40NiCr1Mo15
| Available Properties |
- Density
- Hardness, Knoop
- Hardness, Vickers
- Tensile Strength, Ultimate
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bulk Modulus
- Poissons Ratio
- Machinability
- Shear Modulus
- Electrical Resistivity
- Electrical Resistivity at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|